1 / 10
Hydrogen-induced cracking (HAC) in a weld joint typically occurs
A
Hours to days after welding as hydrogen diffuses and residual stresses are present
B
Only in austenitic stainless steel welds
C
Only in the weld metal, never in the heat-affected zone
D
During welding while the weld pool is still liquid
Check Answer